Cathodic Protection of a Pipeline (overview)

Sacrificial anodes or a rectifier and ground bed push current into a buried pipe.

Loading the animation…
You are watching a free lesson. A free account saves your progress and lets you mark lessons complete. Create a free account Sign in

What cathodic protection does

A buried steel pipeline is wet, salty ground on the outside and a flowing product on the inside. Steel in damp soil slowly turns back into rust. Cathodic protection stops this by using a small direct current. The current is arranged so that it runs into the pipe from the soil, and never out of it. Steel that receives current does not corrode.

Protection works together with a coating on the pipe. The coating does most of the work and the current protects the small places where the coating fails. This lesson is the overview of pipeline integrity. The gas pipeline pigging lesson shows how the inside of the pipe is cleaned and checked, and the crude pipeline station lesson shows the pumps that move the oil. The drawing shows two ways of making the current side by side. A real length of pipe usually has one system or the other.

How it works

  1. 1Corrosion is a current. Wherever bare steel touches wet soil, tiny currents flow. At one spot, the anode, current leaves the steel and iron goes into the soil as ions. This is corrosion. At another spot, the cathode, current enters the steel and nothing is lost. In the first half of the animation, iron leaves the bare steel of a damaged spot.
  2. 2Coating first. A coating on the outside of the pipe keeps soil water away from the steel. Only the small places where it is damaged, called holidays, are open to the soil. That is why a coated pipe needs only a small current, about a thousand times less than a bare pipe would need.
  3. 3Sacrificial anode. A block of magnesium or zinc, metals that corrode more easily than steel, is buried near the pipe in a backfill bag and joined to the pipe by a wire. Current now leaves the block instead of the pipe. The block is slowly eaten away, and the pipe is spared. It needs no power supply.
  4. 4Transformer-rectifier. The second method, impressed current, uses power from the grid. A transformer lowers the voltage and a rectifier turns the alternating current into direct current. The positive terminal is joined to the anodes and the negative terminal to the pipe, so the unit drives the current round the circuit.
  5. 5Ground bed. The anodes of an impressed current system are made of a material that hardly corrodes and are packed in a coke backfill that carries current well. This group of anodes is the ground bed. Current leaves it, crosses the soil and arrives at the holidays of the pipe. The current then returns to the rectifier along the negative cable.
  6. 6Test post and reference electrode. Wires from the pipe are brought up to a test post. To check the protection, a voltmeter is joined between the pipe wire and a reference electrode (a copper rod in copper sulphate solution) standing on the soil above the pipe. The reading is the pipe-to-soil potential. A reading more negative than about −0.85 V on this electrode is typically taken to show that the pipe is protected.

The numbers

Typical features: unprotected steel in soil sits at about −0.5 to −0.6 V against a copper sulphate electrode, and protection moves it more negative, to about −0.85 V or beyond. Too much is harmful too, because a potential much more negative than about −1.2 V can lift the coating. A coated pipe typically needs a few to some tens of microamperes for each square metre of surface, while bare steel in soil typically needs milliamperes, about a thousand times more. Magnesium anodes sit at about −1.5 V and zinc at about −1.1 V against the same electrode. Magnesium typically gives about 1,100 ampere-hours for each kilogram used, and zinc about 780.

Worked example 1, a sacrificial system. Assume a coated pipe 0.3 m across and 2 km long that needs 20 µA for each square metre, a life of 25 years, and anodes that each put out 15 mA.

QuantityWorkingResult
Pipe surfaceπ × 0.3 × 2,000about 1,885 m²
Current needed1,885 × 20 µA37,700 µA, about 37.7 mA
Number of anodes37.7 ÷ 152.5, so 3 anodes
Charge over 25 years0.0377 A × 8,760 h × 25about 8,256 A·h
Magnesium needed8,256 ÷ 1,100about 7.5 kg, so three 5 kg anodes (15 kg) give about twice the minimum

Worked example 2, an impressed current system. Assume a coated pipe 0.5 m across and 20 km long, the same 20 µA for each square metre, twice the current to allow for the coating ageing, and a circuit resistance of 5 Ω (ground bed, cables and soil).

QuantityWorkingResult
Pipe surfaceπ × 0.5 × 20,000about 31,400 m²
Current needed31,416 × 20 µAabout 0.63 A
Design current, with an allowance of 20.63 × 2about 1.26 A
Voltage the unit must give1.26 A × 5 Ωabout 6.3 V
Power6.3 V × 1.26 Aabout 7.9 W
The same pipe if it were bare, at 20 mA for each m²31,416 × 0.020 Aabout 628 A, 1,000 times more

The result shows why the coating matters. A real unit is rated much higher than this first figure, because the coating wears, the soil dries and the ground bed ages.

Assumed inputs, not data from a particular plant. Real designs depend on the coating, the soil resistivity, the pipe and the standards that apply.

Safety: the rectifier is connected to the grid voltage, and the pipe, cables and anodes can carry direct current that can spark if a joint is opened. The line itself may hold flammable gas or oil. Work on these systems is done by trained people with permits and tested equipment. This lesson explains the idea and is not a procedure.

What the operator watches

  • Pipe-to-soil potential. Readings at the test posts, taken at regular intervals, show whether every part of the line is protected.
  • Rectifier output. The voltage and the current of each unit, so a unit that has tripped or drifted is noticed.
  • Anode condition. The current from a sacrificial anode falls as it is used up, and a ground bed slowly wears.
  • Coating condition. Surveys along the line look for holidays, because a growing damaged area needs more current.

Common problems

  • Dry soil. Soil with a high resistance lets less current flow, so the pipe may fall short of protection.
  • Broken connection. A cut cable, a poor weld or a corroded joint stops the current, even though the anode is fine.
  • Stray current. Current from other pipes, railways or power lines can enter the pipe and leave it again somewhere else, and corrode the steel there.
  • Shielding. A coating that has come loose can hold water against the steel and keep the current out.

Words you will meet

Anode
The place where current leaves a metal into the soil. The metal there is the one that is lost.
Cathode
The place where current enters a metal. A protected pipe is made a cathode, so it does not corrode.
Holiday
A bare spot or a flaw in a coating.
Sacrificial anode
A block of a more active metal that is eaten away in place of the pipe.
Impressed current
Protection in which a power supply drives the current instead of a metal.
Ground bed
A group of buried anodes that put the current into the soil.
Reference electrode
An electrode with a steady, known voltage against which a pipe potential is read.
Backfill
Material packed round an anode that keeps it moist and carries the current.

Check your understanding

Why does a coated pipe need so much less current than a bare pipe?

The current only has to protect the steel that the soil can reach. The coating hides almost all of the steel, so only the holidays take current. In the worked example the bare pipe would need about 1,000 times more.

In the sacrificial method, what is being “sacrificed” and where does it go?

The magnesium or zinc block. It dissolves into the soil as ions, and that is the corrosion that would otherwise happen to the pipe. When the block is used up, it must be replaced.

Which terminal of the rectifier is joined to the pipe, and why?

The negative terminal. The pipe must receive current from the soil, and the positive terminal sends current out through the anodes of the ground bed. The current returns along the negative cable.

Key facts

Principle
Make the whole pipe the place where current enters, never leaves.
Two methods
Sacrificial anodes, or impressed current from a rectifier.
Typical check
Pipe-to-soil potential more negative than about −0.85 V against copper sulphate.
First defence
The coating. The current protects only its flaws.
Direction
Current runs from the anodes through the soil to the pipe.
Use the animation
The ground is cut open so the pipe shows as a ring: dark bore, grey steel wall and yellow coating with two bare spots. The numbers on the drawing match the steps under How it works. In the first part of the loop protection is off: orange dots show iron leaving the bare steel, and the meter in the front reads low. In the second part protection is on: the orange dashes show the current running through the soil from the anode on the left and the ground bed on the right to the pipe, and the meter swings into the green. The arrows show the direction of conventional current. Hover over any part for its name and what it does.