Lithium: Spodumene to Hydroxide

From ore to lithium hydroxide: crush, concentrate, calcine, roast, leach, purify.

Loading the animation…
You are watching a free lesson. A free account saves your progress and lets you mark lessons complete. Create a free account Sign in

What a lithium plant does

Australia mines lithium as spodumene, a lithium aluminium silicate found in a coarse rock called pegmatite. The plant concentrates the spodumene, heats it until its crystal structure opens up, and uses acid to turn it into a lithium salt in solution. The solution is cleaned and the lithium chemical is crystallised. Battery makers buy that chemical, most often lithium hydroxide or lithium carbonate. This lesson follows the hydroxide route.

The first part of the animation is a concentrator like the one in the mineral processing plant lesson. The rest is a chemical plant that turns the concentrate into the product. Lithium can also come from brines, which is a different route and is not shown here.

How it works

Each stage makes the lithium richer or easier to reach, and leaves something else behind: waste rock, then residue, then unwanted metals, then sodium sulphate.

  1. 1Mine and crush. The pegmatite ore is mined and broken by a jaw crusher. A conveyor carries it on.
  2. 2Upgrade. Coarse spodumene is picked out by dense media separation in a cyclone. Fine spodumene is floated off in flotation cells. Together they make a concentrate called SC6, typically about 6 percent lithium oxide (Li2O). The waste leaves as tailings to the tailings storage.
  3. 3Calcine. A preheater and a rotary kiln heat the concentrate to typically about 1,000 to 1,100 °C. This changes alpha spodumene, which is hard and unreactive, to beta spodumene, which acid can attack (see the calciner).
  4. 4Acid roast. The beta spodumene is mixed with sulphuric acid and roasted in a second kiln. The lithium becomes water-soluble lithium sulphate (see acid roast and leach).
  5. 5Leach. Water dissolves the lithium sulphate in agitated tanks and leaves solids behind. A filter removes the solids as a residue.
  6. 6Purify. Lime or soda ash neutralises the acid and removes magnesium, calcium, iron and aluminium as solids. A filter press takes them out, and ion exchange columns polish the solution so it is clean.
  7. 7Convert and crystallise. Caustic (sodium hydroxide) turns the solution into lithium hydroxide. An evaporative crystalliser grows the crystals, a centrifuge separates them, and a dryer and bagging make the product. A plant that makes carbonate uses soda ash here instead. See purification and crystallisation.

The numbers

Typical figures; every ore and plant is different. Pure spodumene is about 8.0 percent Li2O, so a concentrate of 6 percent is about 75 percent spodumene (6 ÷ 8.0). The industry counts lithium as lithium carbonate equivalent, LCE: 1 t of Li2O is 2.47 t of LCE. 1 t of Li2O makes about 2.81 t of lithium hydroxide monohydrate.

Worked example. Assume 100 t of SC6 concentrate at 6 percent Li2O and a chemical recovery of 90 percent.

QuantityWorkingResult
Li2O in the concentrate100 × 0.066.0 t
Most LCE6.0 × 2.47314.8 t
LCE at 90 percent14.8 × 0.90about 13.4 t
Most lithium hydroxide monohydrate6.0 × 2.8116.9 t
Hydroxide at 90 percent16.9 × 0.90about 15.2 t
Concentrate per tonne of LCE100 ÷ 13.4about 7.5 t of SC6
Concentrate per tonne of hydroxide100 ÷ 15.2about 6.6 t of SC6

The same Li2O makes more tonnes of hydroxide monohydrate than of carbonate (2.81 against 2.47), because the hydroxide crystal carries more oxygen, hydrogen and water for each lithium. So fewer tonnes of concentrate are needed for each tonne of hydroxide than for each tonne of carbonate.

Assumed inputs, not data from a particular plant.

Safety: kilns, hoods and hot solids are very hot, sulphuric acid and caustic solution burn skin and eyes, and the gases from the roast are harmful, so they are collected and cleaned. Dust from lime, soda ash and lithium hydroxide is an irritant. Protective equipment, closed handling and isolation of equipment are part of the design. This lesson explains the process; it is not a procedure.

What the operator watches

  • Concentrate grade and recovery. Flotation and dense media results set how much lithium reaches the chemical plant.
  • Calciner temperature and conversion. The kiln must turn enough alpha spodumene into beta spodumene.
  • Acid dose, leach solids and pH. They show whether the lithium is being brought into solution.
  • Impurities in the purified solution. Magnesium and calcium must be very low before the crystalliser.
  • Crystalliser temperature and slurry density. They decide the size and purity of the crystals.

Common problems

  • Under-calcined concentrate. If too little beta spodumene forms, lithium does not leach.
  • Sticky roast. A poorly mixed or over-acid feed can cake inside the kiln.
  • Impurity breakthrough. Calcium or magnesium that passes the purification contaminates the crystals.
  • Scaling. Salts coat the heater in the crystalliser and cut its heat transfer.
  • Sodium sulphate. The plant makes a large by-product stream of sodium sulphate that must be handled.

Words you will meet

Spodumene
The lithium mineral, a lithium aluminium silicate.
Pegmatite
The coarse-grained rock that holds the spodumene.
SC6
A spodumene concentrate of about 6 percent Li2O.
Li2O and LCE
Lithium oxide, and lithium carbonate equivalent: two ways to count the lithium.
Alpha and beta spodumene
The hard, unreactive form and the open form that acid can attack.
Calcination
Heating a solid to change its structure without melting it.
Acid roast
Roasting a solid mixed with acid so the lithium turns into a soluble salt.
Battery grade
A purity specification strict enough for battery makers.

Check your understanding

Why is spodumene heated before the acid is added?

Alpha spodumene is unreactive. Heating changes it to beta spodumene, which the acid can dissolve.

Why does the solution need lime or soda ash?

They neutralise the acid and take out unwanted metals such as magnesium, calcium, iron and aluminium.

How much Li2O is in 100 t of SC6 at 6 percent?

100 × 0.06 = 6 t.

Key facts

Concentrate
SC6 is typically about 6 percent Li2O, about 75 percent spodumene.
Calcination
Typically about 1,000 to 1,100 °C, alpha to beta spodumene.
Conversion factors
1 t Li2O is 2.47 t LCE or about 2.81 t lithium hydroxide monohydrate.
Example
100 t of SC6 gives about 15.2 t of hydroxide at 90 percent recovery.
By-product
Sodium sulphate, in large quantity.
Use the animation
The animation is clickable: click the crusher, the conveyor, the cyclone, a flotation cell, the tailings storage, the calciner, the acid roast kiln or leach tanks, the filter, the purification and crystalliser equipment, the dryer or the bags to open its own lesson. Follow the ore along the back row to the flotation cells, then the concentrate to the calciner on the middle row. The solids move from right to left through the acid roast and the leach. The solution then runs along the front row to the crystalliser and the bags. The numbers on the drawing match the numbered steps under How it works. Hover over any part for its name and what it does.